SILIT-2840LV

ʻO ka wehewehe pōkole:

ʻO SILIT-2840LV ka mea hoʻomaʻemaʻe silicone amino a me ka wai silicone reactive, aneane ʻaʻohe d4d5d6 e hoʻokō i nā lula EU hou. Hiki ke hoʻohana ʻia ka huahana i nā ʻano lole lole like ʻole, e like me ka pulupulu, ka hui ʻana o ka pulupulu, He maikaʻi ka palupalu a me ka maʻalahi, ka hopena liʻiliʻi ma ke ʻano o ke keʻokeʻo a me ka drapability.


Huahana Huahana

FAQ

Huahana Huahana

Nā waiwai:
Akaka ka ʻike i ka wai turbid
PH waiwai 7~9
ʻOka, 25 ℃ Ma kahi o 4000mPa•S
Helu Amine Ma kahi o. 0.4
Hoʻohālikelike Hoʻohana ʻia me nā mea kōkua cationic a me nonionic

Nā hiʻohiʻona:
ʻO ka palupalu maikaʻi a me ka maʻalahi.
Maikaʻi drapability

Nā noi:
1 Kaʻina hoʻopau:
SILIT-2840LV(30%emulsion) 0.5~1%owf (Ma hope o ka dilution)
Hoʻohana: 40 ℃ ~ 50 ℃ × 15 ~ 30 min

2 Ke kaʻina hana ʻana:
SILIT-2840LV(30%emulsion) 5~15g/L (Ma hope o ka dilution)
Hoʻohana: pālua-luu-lua-nip
Keʻano emulsification:
SILIT-2840LV<100% maʻiʻo paʻa> emulsified i 30% paʻa maʻiʻo cationic emulsion
SILIT-2840LV----200g
+To5 ----50g
+To7 ----50g
+ Ethylene glycol monobutyl ether ----10g; a laila e hoʻoulu i 10 mau minuke
② +H2O ----200g; a laila e hoʻoulu i 30 mau minuke
③ +HAc (----8g) + H2O (----292); a laila e hoʻohui mālie i ka hui ʻana a me ka hoʻoulu ʻana 15min
④ +H2O ----200g; a laila e hoʻoulu i 15 mau minuke
Ttl.: 1000g / 30% maʻiʻo paʻa
Pūʻolo:
SILIT-2840LVloaʻa i loko o 200kg pahu plastik.

Ka mālama ʻana a me ka mālama ʻana:
Ke mālama ʻia i loko o ka pahu mua i wehe ʻole ʻia ma kahi mahana ma waena o +2°C a +40°C,SILIT-2840LVhiki ke hoʻohana ʻia a hiki i 12 mau mahina ma hope o ka lā o ka hana ʻana i kaha ʻia ma ka pahu (DLU). E mālama i nā ʻōlelo aʻoaʻo no ka mālama ʻana a me ka lā pau i hōʻailona ʻia ma ka pahu. Ua hala keia la,SHANGHAI HONNEUR TECHʻaʻole hōʻoia hou e hoʻokō ka huahana i nā kikoʻī kūʻai.

 

 

 